Thermal reeflective insulation made of one external pure aluminum foil layer covering a single core layer of flame retardant polyethylene bubble film. |
|
|
|
Technical Specification
Property |
Units |
Dir |
Value |
|
|
|
Regular |
Reinforce (AN) |
Nominal thickness |
Mm |
|
4.0 |
Emmisivity (ASTM C 1371) |
|
|
0.05 |
Reflectivity (ASTM C 1371) |
|
|
0.95 |
Heat resistance (R)- under roof |
m2·0C/W |
Down |
1.54 |
Noise Reduction Coefficient (ASTM E-384) % 54% |
% |
|
54% |
Tensile strength @peak (ASTM C-1136) |
g/cm-width |
MD |
2500 |
4480 |
TD |
2400 |
5000 |
Elongation†@peak (ASTM C-1136) |
% |
MD |
18.7 |
15.0 |
TD |
12.0 |
10.0 |
Tear strength (ASTM D-1938) |
N |
MD |
13.0 |
20.0 |
TD |
15.0 |
20.0 |
Classification of Reaction to Fire** (IS 755) |
|
|
Class II 3.2 |
Water Vapor Transmission (ASTM E-96) |
g /ft2·hr |
|
0.018 (method A) |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Corrosion Resistance (Internal Test) |
Conc.HCl |
|
High Resistance* |
Yield (Nominal) |
g/m2 |
|
230 |
249 |
Standard Roll Size |
m x m |
|
1.17x57 |
1.2x30 |
Standard Roll Weight (Gross) |
kg |
|
±15.3 |
±17.0 |
|
 |
|
Thermal reflective insulation made of two external pure aluminum foil layers covering a single core layer of polyethylene bubble film. |
|
|
|
Technical Specification
Property |
Units |
Dir |
Value |
|
|
|
Regular |
Reinforce (AN) |
Nominal thickness |
mm |
|
3.8 |
Emmisivity (ASTM C 1371) |
|
|
0.05 |
Reflectivity (ASTM C 1371) |
|
|
0.95 |
Heat resistance (R)-under roof |
m2·0C/W |
Down |
2.98 |
Noise Reduction Coefficient (ASTM E-384) |
% |
|
54% |
Tensile strength @peak (ASTM C-1336) |
g/cm-width |
MD |
2200 |
5800 |
TD |
2500 |
7100 |
Elongation @peak (ASTM D-882) |
% |
MD |
18.7 |
15 |
TD |
10.0 |
10 |
Tear strength (ASTM D-1004) |
N |
MD |
11.0 |
22 |
TD |
15.0 |
20 |
Puncture resistance (TAPPI T 803) |
Joule |
|
5.3 |
5.3 |
Classement de Réaction Au Feu*** |
|
|
M1 |
Classification of Reaction to Fire** (EN 13501-1:2002) |
|
|
Euroclass B-s2,d0 |
Water Vapor Transmission(ASTM E-96) |
g /ft2·hr |
|
0.018 (method A) |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Corrosion Resistance (Internal Test) |
Conc.HCl |
|
High Resistance* |
Yield (nominal) |
g/m2 |
|
225 |
240 |
Standard Roll Size |
m x m |
|
1.17x57 |
1.2x57 |
Standard Roll Weight (Gross) |
kg |
|
±15 |
±16.4 |
* All products are supplied with high resistance (H.R.) treatment against corrosion as standard.
** Tested in accordance to the new European Community standard by WFRC (Report Ref.E141990)
*** Based on procès verbal No. 10512-02 by SNPE Propulsion - Laboratoire d'Essais au Feu |
 |
|
Thermal reflective insulation made of two external pure aluminum foil layers covering a double core layer of polyethylene bubble film. |
|
|
|
Technical Specification
Property |
Units |
Dir |
Value |
Nominal thickness |
mm |
Down |
8 |
Emmisivity (ASTM C 1371) |
|
|
0.05 |
Reflectivity (ASTM C 1371) |
|
|
0.95 |
Heat resistance (R)-under roof |
m2·0C/W |
|
3.06 |
Noise Reduction Coefficient (ASTM E-384) |
% |
|
55% |
Sound Transmission Class (ISO 171-1) |
dB |
|
-6 |
Tensile strength @peak (ASTM C-1136) |
g/cm-width |
MD |
2650 |
TD |
2750 |
Elongation @peak (ASTM C-1136) |
% |
MD |
18.7 |
TD |
18 |
Tear strength (ASTM D-1938) |
N |
MD |
12.5 |
TD |
13.5 |
Puncture resistance (TAPPI T 803) |
Joule |
|
4 |
Surface Flame Spread ** (BS 476:Part 7) |
|
|
Class 1 |
Water Vapor Transmission (ASTM E-96) |
g/ft2·hr |
|
0.018 (method A) |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Corrosion Resistance (Internal Test) |
Conc.HCl |
|
High Resistance * |
Yield (nominal) |
g/m2 |
|
320 |
Standard Roll Size |
m x m |
|
1.20 x 40 |
Standard Roll Weight (Gross) |
kg |
|
±15.4 |
* All products are supplied with high resistance (H.R.) treatment against corrosion as standard.
** Tested by Warrington Fire Research Centre Ltd. U.K. (Test Report No.121611) |
|
 |
|
Vapor barrier made of two external pure aluminum foil layers covering a reinforcing net in the middle. |
|
|
|
Property |
Units |
Dir |
Value |
|
|
|
Regular |
Reinforce (AN) |
Nominal thickness |
mm |
|
0.12 |
Emmisivity (ASTM C 1371) |
|
|
0.05 |
Reflectivity (ASTM C 1371) |
|
|
0.95 |
Heat resistance (R) - under roof |
m2·0C/W |
Down |
1.44 |
Tensile strength @peak (ASTM C-1336) |
g/cm-width |
MD |
2700 |
7000 |
TD |
2600 |
7800 |
Dimensional changes at high Temp (ASTM D-1204) |
% |
MD |
-0.06 |
-0.03 |
TD |
-0.13 |
-0.05 |
Puncture resistance (TAPPI T 803) |
Joule |
|
0.7 |
1.6 |
Thermal Integrity of Vapor Barrier (ASTM C-1263) |
@-29ºC to +60ºC |
MD |
No cracks |
TD |
No delamination |
Surface Burning Characteristics** (ASTM E-84 Equiv.UL723) |
|
|
Class A
[Flame=20 /Smoke=60] |
Classification of Reaction to Fire ***(EN 13501-1:2002) |
|
|
Euroclass B-s2, d0 |
Moisture Vapor Transmission Rate (TNO/PIRA @38°C,90%R.H.) |
g/m2 day |
|
0.001 |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Corrosion Resistance (Internal Test) |
Conc.HCl |
|
High Resistance* |
Yield (nominal) |
g/m2 |
|
140 |
155 |
Standard Roll Size |
m x m |
|
1.2x100 |
1.2x100 |
Standard Roll Weight (Gross) |
kg |
|
±16.8 |
±18.6 |
* All products are supplied with high resistance (H.R.) treatment against corrosion as standard.
** Tested by SGS U.S. Testing Company Inc. (Report No. 740979-1)
*** Tested in accordance to the new European Community standard by WFRC (Report Ref.E141990) |
|
 |
|
Thermal reflective insulation made of two external pure aluminum foil layers covering a single core layer of large polyethylene bubble film. |
|
|
|
Technical Specification
Property |
Units |
Dir |
Value |
|
|
|
Regular |
Reinforce (AN) |
Nominal thickness |
Mm |
|
8.0 |
Emmisivity (ASTM C 1371) |
|
|
0.05 |
Reflectivity (ASTM C 1371) |
|
|
0.95 |
Heat resistance (R) - under roof |
m2·0C/W |
Down |
3.06 |
Noise Reduction Coefficient (ASTM E-384) % 55% |
|
|
55% |
Tensile strength @peak (ASTM C-1336) |
g/cm-width
|
MD |
2500 |
4400 |
TD |
2200 |
6000 |
Elongation†@peak (ASTM C-1336) |
%
|
MD |
18.7 |
12.5 |
TD |
7.6 |
10.5 |
Tear strength (ASTM C-1938) |
N
|
MD |
9.6 |
20.0 |
TD |
12.1 |
20.0 |
Puncture resistance (TAPPI T 803) |
Joule |
|
3.5 |
7.1 |
Surface Flame Spread** (BS 476 :Part 7) |
|
|
Class 1 |
Water Vapor Transmission (ASTM E-96) |
g /ft2·hr |
|
0.018 (method A) |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Corrosion Resistance (Internal Test) |
Conc.HCl |
|
High Resistance* |
Yield (nominal) |
g/m2 |
|
225 |
240 |
Standard Roll Size |
m x m |
|
1.17x30 |
1.2x30 |
Standard Roll Weight (Gross) |
kg |
|
±7.8 |
±8.6 |
|
 |
|
Thermal and Acoustic Reflective insulation made of two pure aluminum foil layers covering a single or double core layer of large bubble film specially formulated for increased acoustic attenuation. |
|
|
|
Technical Specification
Property |
Units |
Dir |
Value |
|
|
|
1kg/m2 |
2kg/m2 |
Nominal thickness |
Mm |
|
9 |
17 |
Emmisivity (ASTM C 1371) |
|
|
0.05 |
Reflectivity (ASTM C 1371) |
|
|
0.09 |
Heat resistance (R)-under roof |
m2·0C/W |
Down |
3.06 |
3.16 |
Heat resistance (R)-wall cavity |
m2·0C/W |
Horiz |
1.69 |
1.81 |
Sound Transmission Class ISO 717-1 |
dB perp. |
|
-11 |
-16 |
System STC Range (Inside Measurment) |
dB |
out ► in |
-20 to -50 |
Surface Flame Spread* (BS 476 :Part 7) |
|
|
Class I |
Water Vapor Transmission (ASTM E-96) |
g /ft2·hr |
|
0.018 (method A) |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Yield (nominal) |
g/m2 |
|
1000 |
2000 |
Standard Roll Size / Sheet Size |
m x m |
|
1.2x15 |
1.2x2.5 |
Standard Roll Weight (Gross) |
kg |
|
±18 |
6.0 |
* Tested by Warrington Fire Research Centre Ltd. U.K. (Test Report No.121611) |
 |
|
Reflective insulation made of two external pure aluminum foil layers covering a double core layer of large bubble film encasing additional reflective surfaces inside the airtight cells. |
|
|
|
Technical Specification
Property |
Units |
Dir |
Value |
Emmisivity* (ASTM C 1371) |
|
|
0.05 |
Reflectivity* (ASTM C 1371) |
|
|
0.95 |
Nominal thickness: |
|
MM |
16.0 |
Heat resistance (R)** - under roof (ASTM C 1363) |
m2·0C/W |
Down |
3.72 |
Heat resistance (R)** - under roof (ASTM C 1363) |
m2·0C/W |
Up |
1.46 |
Heat resistance (R) - wall caviey |
m2·0C/W |
Horiz. |
2.10 |
Noise Reduction Coefficient (ASTM E-384) |
% |
|
55% |
Tensile strength @peak (ASTM C-1136) |
g/cm-width
|
MD |
4200 |
TD |
4000 |
Tear strength (ASTM D-1938) |
N
|
MD |
15.0 |
TD |
15.0 |
Puncture resistance (TAPPI T 803) |
Joule |
|
4.5 |
Surface Flame Spread*** (BS 476 :Part 7) |
|
|
Class 1 |
Water Vapor Transmission (ASTM E-96) |
g /ft2·hr |
|
0.018 (method A) |
Fungal Resistance Test (ASTM C 1338) |
|
|
No fungal growth |
Yield (nominal) |
g/m2 |
|
336 |
Standard Roll Size |
m x m |
|
1.2x20 |
Standard Roll Weight (Gross) |
kg |
|
±8.4 |
|
|
|